MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
348H Austenitic Stainless Steel, UNS S34809
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/ccType 348
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 195 GPaType 348
Poissons Ratio 0.27Type 348
Shear Modulus 77.0 GPaType 348
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000791 ohm-cm
@Temperature 20.0 °C
Type 348
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.3 µm/m-°C
@Temperature 0.000 - 100 °C
Type 348
 17.8 µm/m-°C
@Temperature 0.000 - 260 °C
Type 348
 18.4 µm/m-°C
@Temperature 0.000 - 540 °C
Type 348
 18.7 µm/m-°C
@Temperature 0.000 - 650 °C
Type 348
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Type 348
Thermal Conductivity 16.3 W/m-K
@Temperature 100 °C
Type 348
 21.5 W/m-K
@Temperature 500 °C
Type 348
Melting Point 1400 - 1425 °CType 348
Solidus 1400 °CType 348
Liquidus 1425 °CType 348
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.04 - 0.10 %
Chromium, Cr 18 %
Iron, Fe 70 %As Balance
Nb + Ta <= 1.0 %Nb + Ta Minimum = 8 x C
Nickel, Ni 11 %
Tantalum, Ta <= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
347 Stainless Steel, annealed
348 Stainless Steel, annealed
347 Stainless Steel, annealed, plate
348 Stainless Steel, annealed, plate
321H Austenitic Stainless Steel (UNS S32109)

MQ348H / 172236

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.