PRE-ELEC PPE 1462 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PPE 1462 has an excellent balance of mechanical properties and is easy to injection mould. Typical applications include injection molded IC-trays and technical parts where a high heat resistance is needed. Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod. Information provided by Premix Thermoplastics Inc. |