MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Arkema Lacovyl® RB 8010 PVC  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: LACOVYL RB 8010 is a low molecular weight vinyl chloride homopolymer.

Its characteristics are :

  • Viscosity index (ISO 1628-2):80 ml/g,(K value:57). Apparent density (ISO 60):0.62 g/ml.
  • ease of fusion and good flow characteristics in the molten state facilitating low temperature processing.
  • good porosity and high apparent density providing high productivity in compound mixers and extruders.
  • high level of purity due to the mass polymerization process giving finished products of very good transparency.
  • a narrow range of particle size distribution.

* RECOMMENDED APPLICATIONS

  • Provides finished products of high transparency, good gloss and free from fish eyes by:
  • calendering and extrusion of rigid sheets and films.
  • extrusion and injection blow-molding of bottles.
  • Injection molding of rigid parts.
  • Extrusion of small rigid profiles and monofilaments.
  • Production of powder coatings by the fluidization method.
  • Molding of gramophone records (Addition resin).

* EXAMPLES OF APPLICATION

  • NAKAN RMA 705 N NAKAN RMS 501 L NAKAN RRS 40

ISO data provided by the manufacturer, Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Number 80 cm³/g
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 80 %Mfr. reports 'Transparent' but doesn't quantify.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Lacovyl® RB 8010 M PVC
Arkema Lacovyl® PE 1311 H PVC
Formosa Plastics Formolon® 680 PVC
Arkema Lacovyl® PE 1801 H PVC
Arkema Lacovyl® PE 1312 PVC

PZARKG297 / 25591

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.