Notes: Sarlink ML-1100 is a general purpose thermoplastic elastomer series, available in NAT and BLK, designed for automotive interior applications. Sarlink ML-1140N NAT is a high hardness, high density, filled grade suitable for injection molding. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Chemical Resistant; Filled; Good Adhesion; Good Flexibility; Good Moldability; Good Tear Strength; Good Toughness; High Density; High Flow; High Specific Gravity; High Hardness; Resilient Uses: Automotive Applications; Automotive Interior Parts; Flexible Grips; General Purpose; Grommets; Knobs; Rubber Replacement; Soft Touch Applications RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding Preliminary data. Information provided by Teknor Apex |