MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound DFL34E Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP LUBRICOMP DFL34E compound is based on Polycarbonate (PC) resin containing 20% glass fiber, 15% PTFE. Added features of this grade include: Wear Resistant, Easy Molding.

Features: Wear resistant,Easy Molding

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/ccASTM D792
Density 1.47 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
 0.0900 %23°C/50% RH/24 hrs; ASTM D570
 0.130 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0030 - 0.0060 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 93.0 MPa5 mm/min; ISO 527
 95.0 MPa5 mm/min; ASTM D638
Elongation at Break 2.7 %5 mm/min; ASTM D638
 3.1 %5 mm/min; ISO 527
Elongation at Yield 2.8 %5 mm/min; ISO 527
Tensile Modulus 6650 MPa1 mm/min; ISO 527
 7190 MPa50 mm/min; ASTM D638
Flexural Strength 145 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
 150 MPaISO 178
Flexural Modulus 6190 MPa2 mm/min; ISO 178
 6320 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 149 JASTM D256
Izod Impact, Unnotched 740 J/mASTM D4812
Izod Impact, Notched (ISO) 13.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 48.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 19.0 JASTM D3763
Impact Test 6.00 JMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.46ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.50ASTM D3702 Modified: Manual
K (wear) Factor 13.0 x 10-10 in³-min/ft-lb-hrRing; ASTM D3702 Modified: Manual
 89.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 175 - 250 VUL 746A
Hot Wire Ignition, HWI >= 120 sec
@Thickness 3.00 mm
UL 746A
High Amp Arc Ignition, HAI 30 - 60 arcs
@Thickness 3.00 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 37.4 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
CTE, linear, Transverse to Flow 63.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 146 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 146 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 141 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 142 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Flammability, UL94 V-1
@Thickness >=3.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 310 - 320 °C
Zone 3 320 - 330 °C
Melt Temperature 305 - 325 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80709 / 288656

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.