MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. This product is available in Natural & Black.

Key Properties: UL94 V0 at 0.8mm and Excellent filling qualities

Benefits: This Red Phosphorous flame retardent grade provides robust UL 94 V-0 and a full UL yellow card while offering good mechanical properties. This grade is suitable for moulding insulating parts for electrical devices, and more generally for thin parts under stress.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/E.C.This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications

Applications: Industrial controls and electrical insulation system

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccISO 1183/A
Water Absorption 0.75 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Viscosity 110 cP
@Shear Rate 1000 1/s,
Temperature 300 °C
 200 cP
@Shear Rate 1000 1/s,
Temperature 280 °C
 200 cP
@Shear Rate 100 1/s,
Temperature 300 °C
 300 cP
@Shear Rate 100 1/s,
Temperature 280 °C
Linear Mold Shrinkage 0.0055 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0050 cm/cm
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 140 MPaISO 527 Type 1A
Tensile Stress at Strain 30.0 MPa
@Strain 0.5 %
 95.0 MPa
@Strain 1 %
 130 MPa
@Strain 1.5 %
 150 MPa
@Strain 2 %
 170 MPa
@Strain 2.5 %
Elongation at Break 2.0 %ISO 527 Type 1A
Tensile Modulus 9000 MPaISO 527 Type 1A
Flexural Strength 250 MPaISO 178
Flexural Modulus 7500 MPaISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²ISO 180/1A
Charpy Impact Unnotched 50.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 3.4IEC 60250
Dielectric Strength 25.0 kV/mmIEC 60243
Dissipation Factor 0.020IEC 60250
Comparative Tracking Index 250 VSolution B; IEC 60112
 300 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.7 µin/in-°F
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 263 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO 75/Af
Flammability, UL94 V-0
@Thickness 0.800 mm
ISO 1210
 V-0
@Thickness 1.60 mm
ISO 1210
 V-0
@Thickness 3.20 mm
ISO 1210
Oxygen Index 30.5 %ISO 4589
Glow Wire Ignition Temperature 725 °CISO 60695-2-13
Glow Wire Flammability Index 960 °CISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 270 - 275 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone275-280°C
Fire and smoke F indexI3/F3NF F 16 101
Mixing Zone280-285°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo Technyl® C216V30 30% Glass Filled Nylon 6
Domo TECHNYL® A 20 V25 PA66, 25% glass fiber, Conditioned
Domo TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY
Domo TECHNYL® C 216 V30 PA6, 30% glass fiber, DRY
Domo TECHNYL® 2411GF6 PA66, 30% glass fiber, DRY

PRHOD584 / 137815

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.