MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Radici Heraflex® E 3918 TPC-ET Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: TPC-ET Thermoplastic Elastomer. Lowest Modulus, Nominal Shore D/15s 35. Natural color

Processing technology: Injection molding

Information provided by Radici group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/cc
Water Absorption 0.73 %
@Time 86400 sec
MI / 08
Melt Flow 34 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 39Instantaneous; ISO 868
 35
@Time 15.0 sec
ISO 868
Tensile Strength at Break 26.0 MPaISO 527-1/2
Elongation at Break 968 %ISO 527 1/2
Flexural Modulus 59.0 MPaISO 178/1A
Izod Impact, Notched NBASTM D256
Tear Strength 113 kN/mASTM D1004
Abrasion 26mm3; DIN 53516
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
Melting Point 180 °C
Vicat Softening Point 128 °C
@Load 5.10 kg
50°C/h
Flammability, UL94 HB
@Thickness 1.60 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hytrel® G3548 NC010 TPC-ET
Radici Heraflex® A 40-11-91 TPS-SEBS Thermoplastic Elastomer
Celanese Hytrel® 3046 NC010 TPC-ET
Celanese Hytrel® 4056 TPC-ET
Celanese Hytrel® 3078 TPC-ET

PRADI750 / 120263

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.