MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Envalior Novamid® ST120 NAT PA6-I
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Impact Modified, Injection Molding

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccdry; ISO 1183
Moisture Absorption 2.80 %Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.015 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.020 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 45.0 MPadry; ISO 527-1/-2
Elongation at Break 30 %dry; ISO 527-1/-2
 >= 50 %cond; ISO 527-1/-2
Elongation at Yield 4.2 %dry; ISO 527-1/-2
Tensile Modulus 1.90 GPadry; ISO 527-1/-2
Flexural Strength 60.0 MPadry; ISO 178
Flexural Modulus 1700 MPadry; ISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
cond; ISO 179/1eU
 NB
@Temperature 23.0 °C
dry; ISO 179/1eU
Charpy Impact, Notched 42.0 kJ/m²
@Temperature 23.0 °C
dry; ISO 179/1eA
 NB
@Temperature 23.0 °C
cond; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 9.00e+14 ohm-cmdry; IEC 60093
Surface Resistance 3.00e+13 ohmcond; IEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
dry; IEC 60250
 4.0
@Frequency 100 Hz
dry; IEC 60250
Dielectric Strength 29.0 kV/mmdry; IEC 60243-1
Dissipation Factor 0.010
@Frequency 100 Hz
dry; IEC 60250
 0.018
@Frequency 1e+6 Hz
dry; IEC 60250
Comparative Tracking Index 600 Vdry; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°Cdry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°Cdry; ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °Cdry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °Cdry; ISO 75-1/-2
Flammability, UL94 HB
@Thickness 0.800 mm
dry; IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
China Tungsten ST1265 PM Antifriction Parts
AISI 1017 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24
AISI 1017 Steel, cold drawn
China Tungsten ST1260 PM Antifriction Parts

PDSM9834 / 161455

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.