MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CoorsTek Reaction Bonded Silicon Carbide, SCRB (SC-2)
Categories: Ceramic; Carbide

Material Notes: Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a sharp decrease in the flexural strength of the sample.

Information provided by CoorsTek.

Key Words: SiC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.10 g/ccASTM C20
Water Absorption 0.00 %ASTM C373
Particle Size 12 µmAverage Crystal Size - Thin Section Test
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 24.51000 g load
Tensile Strength, Ultimate 307 MPaACMA Test #4
Modulus of Elasticity 393 GPaASTM C848
Flexural Strength 462 MPaASTM F417
Compressive Strength 2500 MPaASTM C773
Poissons Ratio 0.19ASTM C848
Fracture Toughness 4.00 - 5.00 MPa-m½
Shear Modulus 165 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 1000 ohm-cm
@Temperature 500 °C
 <= 1000 ohm-cm
@Temperature 1000 °C
 <= 1000 ohm-cm
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.30 µm/m-°C
@Temperature 25.0 - 1000 °C
ASTM C372
Specific Heat Capacity 0.700 J/g-°CASTM E1269
Thermal Conductivity 125 W/m-KASTM C408
Maximum Service Temperature, Air 1400 °CNo Load
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 0.00 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CoorsTek UltraSiC™ SC-30 Direct Sintered Silicon Carbide
CoorsTek ACI-Co10 Tungsten Carbide
CoorsTek Nitrogen Bonded Silicon Carbide, SCNB
3M Techical Ceramics MYCROSINT® CD Boron Nitride
CoorsTek ACI-Co6 Tungsten Carbide

CZ3C1 / 2745

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.