MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient PolyOne® 15020 White PEC Polyethylene  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: 15020 White PEC concentrate is designed for general purpose extrusion applications, including injection molding, blow molding, and film. The pigment and resin have been selected for compatibility with all polyolefin resins (LDPE, LLDPE, HDPE, and PP).

Description/Features:

  • White
  • General Purpose Grade

Market:

  • Film

Processing Method:

  • Blown Film
  • Cast Film
  • Blow Molding
  • Extrusion

Note: Acceptable for FDA applications depending on end use.

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow >= 9.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Procedure A - Manual Operation; ASTM D1238
 
Descriptive Properties
Base ResinLinear Low Density Polyethylene
Loading50 %
PigmentRutile Titanium Dioxide
Product FormUnderwater Cut Pellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient PolyOne® 15077 White PEC Polyethylene
Avient PolyOne® 1005 White PEC Polyethylene
Avient PolyOne® 1601 Blue PEC Polyethylene
Avient PolyOne® 1006 White PEC Polyethylene
A. Schulman POLYBATCH™ Bright White LL80250 Concentrate Based In LLDPE

PH1PO3386 / 45051

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.