MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Michelman® Michem ® Flex HS9020 Water-based Heat Seal Coating
Categories: Fluid; Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Water-based heat seal coating for heat-sensitive and high-speed packaging lines. Michem® Flex HS9020 may need a primer like Michem® Prime 2300 to adhere to a film substrate. Apply 2 dry gsm meter for best results. For lower COF and anti-block control, use Michem® Lube 160 RPH at 3-5% loading. Usage: A water-based heat seal coating designed for heat sealing with a variety of substrates over a wide temperature range. It is excellent for sealing through contamination and ideal for horizontal and vertical form fill seal applications that require high speeds, have temperature sensitive products, or have products that can contaminate seal areas. Michem® Flex HS9020 has a low seal initiation temperature for improved hot tack performance.

Applications (properties imparted): Heat Seal Coatings (Substrate - film, Substrate - paper, metal).

Handling: Handle in accordance with good industrial hygiene and safety practice. Use personal protective equipment as required.

Information provided by Michelman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 - 0.990 g/cc
Solids Content 24.2 - 25.2 %Non-Volatiles
pH 8.5 - 9.5
Brookfield Viscosity 50 - 400 cPSpindle #2. 60 RPM.
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 MonthDry, cool and well-ventilated place
 
Descriptive Properties
AppearanceTranslucent liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WMICHE9824 / 287419

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.