MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Chemours Teflon® C PFA Grade 560 Static Dissipating Semiconductive Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: Teflon® C PFA resins are available in 2.5-mm (0.1-in.) pellets. These fluoropolymer resins (perfluoroalkoxy) combine the chemical and hightemperature resistance of Teflon® PFA with antistatic levels of electrical conductivity.

Properly processed products made from Teflon® C PFA resins provide the superior properties typical of the fluoropolymer resins: retention of properties after service at 260°C (500°F), useful properties at –196°C (–320°F), and chemical inertness to nearly all industrial chemicals and solvents. Molded products have moderate stiffness, excellent toughness, low coefficient of friction, nonstick characteristics, resistance to creep at high service temperatures, and excellent weather resistance.

These resins can be processed by traditional extrusion and molding processes. They have high melt strength and thermal stability at high processing temperatures.

Three grades of Teflon® C PFA resins covering a broad range of Melt Flow Rates (MFR) are available. The low MFR resin provides a higher degree of stress crack resistance while the high MFR resin is easier to process.

Applications

Applications for Teflon® C PFA include extruded tubing, pipe, and other profiles for hose; linings of components used in the chemical processing industries; industrial film; and injection- and blowmolded articles requiring superior electrical, chemical, and thermal properties.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.12 - 2.17 g/ccASTM D792
Melt Flow 7.6 g/10 minASTM D3307
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ASTM D2240
Tensile Strength, Ultimate 17.0 MPaASTM D3307
Elongation at Break 250 %ASTM D3307
Izod Impact, Notched NBASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.0 - 10 ohm-cmASTM D257
Arc Resistance >= 180 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Melting Point 302 - 310 °CASTM D3418
Maximum Service Temperature, Air 260 °C
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Processing Temperature 379 - 399 °CCure Temperature
 
Descriptive Properties
Heat of Combustion J/g5300ASTM D240

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Teflon® PFA Grade 440 HP Extrusion and Molding Resin
Chemours Teflon® PFA Grade 345T Extrusion and Molding Resin for High Temperature Applications
Chemours Teflon® C PFA Grade 510 Static Dissipating Semiconductive Resin
Celanese FORTRON® 1140 E7 Polyphenylene Sulfide (PPS)

PDU9227 / 33340

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.