MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kangxi Plastics FRHIPSMIV-0 HIPS, Flame Retardant
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Applications: Television shell, sound shell, shell of electronic injection molding products

Modified Features: Flame retardant

Product Features: Apply to gas assisted injection molding , comply with ROHS, good comprehensive performance, good heat stability and electrical property, and flame retardant grade is UL-94 V0

Information provided by Wuxi Kangxi Plastics Technology Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 25.0 MPa50mm/min; ASTM D638
Elongation at Break 30 %50mm/min; ASTM D638
Flexural Strength 35.0 MPa2mm/min; ASTM D720
Flexural Modulus 2100 MPa2mm/min; ASTM D720
Izod Impact, Notched 100 J/m
@Thickness 3.20 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 80.0 °C
@Thickness 2.00 mm
IEC695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
@Thickness 6.40 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
@Thickness 6.40 mm
ASTM D648
Flammability, UL94 V-0
@Thickness 1.60 mm
 V-0
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Front Barrel Temperature 180 - 230 °C
Melt Temperature 220 - 245 °C
Mold Temperature 30.0 - 60.0 °C
Drying Temperature 70.0 °C
Dry Time 2.00 hour
 
Descriptive Properties
Weather Resistant0.000424hr, ASTM D570

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKXP015 / 281791

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.