MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger Tecapeek® UD Blue Ultra Detectable Polyetheretherketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Tecapeek® UD Blue is an Ultra Detectable PEEK (metal- and x-ray-detectable).

Target Industries:

  • food processing
  • engineering for beverage filling systems
  • pharmaceutical industry
  • heat exchanger
  • conveyor technology

Information provided by Ensinger Special Polymers, Inc.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.74 g/ccASTM D790
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 101ASTM D785
Tensile Strength 12750 psiASTM D638
Elongation at Break 4.13 %ASTM D638
Elongation at Yield 3.43 %ASTM D638
Tensile Modulus 772200 psiASTM D638
Flexural Strength 21230 psiASTM D790
Flexural Modulus 728400 psiASTM D790
Compressive Strength 21240 psiat 10% deformation; ASTM D695
Compressive Modulus 536700 psiASTM D695
Izod Impact, Notched 0.790 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 644 °FASTM D3418
Maximum Service Temperature, Air 500 °FLong Term; UL746B
 572 °FShort Term
 
Descriptive Properties
ColorDark Blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger Tecapeek® Polyetheretherketone (PEEK)
Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK)
Ensinger Tecapeek® PVX Polyetheretherketone (PEEK)
Ensinger Tecapeek® XP-96BST Compression Molded PEEK ST, Unfilled
Mitsubishi Chemical Advanced Materials Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet)

PENSIN999e / 193515

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.