MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NAECO® ELKON® 100W Pure Tungsten
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy; Pure Element

Material Notes: Tungsten, also called Wolfram, occurs as an impure tungsten oxide in wolframite and scheelite ores. It is chemically extracted, refined to an oxide of high purity and reduced to tungsten powder in hydrogen atmosphere furnaces. It is fabricated into wrought metal rods by pressing the powder into ingots, sintering at very high temperatures followed by rolling and swaging. Discs are cut from the rods with abrasive wheels, polished by abrasive tumbling, cleaned and brazed to nickel plated steel backings to form electrical contacts. ELKON® 100W tungsten has a fine grain cold worked structure. The structure is the result of the above method of manufacture. The smaller diameter materials will exhibit finer grain structures than larger materials due to the differences in the total amount of work required to reach the final dimension.

Tungsten has many unique properties that contribute to its outstanding performance as an electrical contact. It has very high melting and boiling temperatures, high density, and equates electrical and thermal conductivity. These properties provide it with excellent resistance to sticking or welding, and outstanding resistance to metal transfer and electrical erosion caused by arcing. Its high hardness and strength make it highly resistant to mechanical wear and deformation where the contacts operate with high closed forces and at high repetitive rates.

In high humidity atmospheres, tungsten is susceptible to electrochemical corrosion. The corrosion results from a cell action when the tungsten is in contact with an active dissimilar metal such as the copper brazing material which is used to attach the tungsten to its backing. The deposits may be quite heavy to the degree that they completely insulate the contacts. A solution to this problem is to braze the tungsten to backings with a less active solder material such as a silver alloy

Tungsten contacts are limited to about 5 amperes in the current that they can normally carry and switch. This is due to their higher contact resistance and oxidation characteristics. At this current level they are usually provided with closed forces of 2 to 4 pounds and an electrical potential of several volts to insure establishing reliable contact. Tungsten contacts are selected for applications where low arc erosion and anti-weld characteristics are important.

Some of the applications include vibrating devices such as automotive horn, magneto ignition and motor speed governor contacts. In other applications, tungsten is selected only for its high resistance to arc erosion. Examples of these arcing applications are furnace igniters and spark gap electrodes.

Tungsten is used as a negative contact paired with CMW's ELKONIUM 33 or ELKONIUM 41 alloys in low voltage DC applications such as automotive voltage regulators or small motor speed governors. In these applications, the contacts operate at highly repetitive rates and the polarized combination is used to maintain a low contact resistance and minimize metal transfer and contact sticking.

Due to its unique properties tungsten is used in many applications other than electrical contacts. Because of its high density it has been used for weights and radiation shielding. Due to its high hardness and good thermal conductivity it has been used for wear surfaces. It can be found in semi-conductor bases and glass seals because of its low thermal expansion and for applications where low arc erosion and anti-weld characteristics are important. Some of the applications include vibrating devices such as automotive horn, magneto ignition and motor speed governor contacts. In other applications, tungsten Refractory Metals, Series 700 and High Density Tooling, Series 800). CMW's engineering can help with many application needs.

Information provided by NAECO, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 19.3 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell A 70
Tensile Strength, Ultimate 827 MPa
Modulus of Elasticity 406 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000550 ohm-cm31% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.43 µm/m-°C
@Temperature 100 °C
Thermal Conductivity 166 W/m-K
Melting Point 3410 °C
Boiling Point 5900 °C
 
Component Elements PropertiesOriginal ValueComments
Tungsten, W 100 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Astaras Anviloy® Weld Rod
Acerde Tungsten
MarkeTech Magnesium Oxide (MgO) Single Crystal Substrate
Zirconium Carbide, ZrC
Acerde Tantalum Carbide

NCMV878 / 192362

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.