MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ScanTube ETFE Tubing
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes:

Information provided by ScanTube, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.73 g/ccASTM D792
Water Absorption <= 0.030 %ASTM D257
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75ASTM D2240
Tensile Strength 6500 psiASTM D638, ASTM D1708
Elongation at Break 200 %ASTM D638, ASTM D1708
Tensile Modulus 120 ksiASTM D638
Flexural Modulus 200 ksiASTM D790
Compressive Strength 7000 psiASTM D695
Izod Impact, Notched NBASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.6
@Frequency 1e+6 Hz
ASTM D150
 2.6
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 2000 V/milShort Term; 10 mil film; ASTM D149
Dissipation Factor 0.00080
@Frequency 1000 Hz
ASTM D150
 0.0050
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.60 BTU-in/hr-ft²-°FASTM C177
Melting Point 260 °C
Maximum Service Temperature, Air 150 °CContinuous
Deflection Temperature at 0.46 MPa (66 psi) 104 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °CASTM D648
Flammability, UL94 V-0
Oxygen Index >= 30 %ASTM D2863
 
Descriptive Properties
Chemical ResistanceExcellent
Weather ResistanceExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zeus ETFE Tubing and Drawn Fiber
Overview of materials for Modified ETFE, Unreinforced
Shanghai Ofluorine J-2 PVDF Extrusion Grade
Shanghai Ofluorine 9201 PVDF Pellets for cables
LNP Thermocomp® FP-EC-1004 Ethylene Tetrafluoroethylene Copolymer, Carbon Fiber Reinforcement

PSCANT905 / 178053

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.