MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
BorsodChem ONGRONOX INP 75 D peroxide-type initiator
Categories: Other Engineering Material; Catalyst/Initiator; Polymer

Material Notes: Chemical name: Bis-(3,5,5-trimethyl-hexanoyl)-peroxide, or Di-isononanoyl-peroxide.
Mol. wt: 314.50 g/mol.
Active oxygen content: 5.09 %.
Deflegmation material: isododecane.
Major decomposition products: carbon-dioxide, 3,3,5-trimethyl-hexanoic acid, 2,4,4-trimethyl-pentane, 2,2,4,7,9,9-hexamethyl-decane, 2`,4`,4`-trimethyl-pentil-3,5,5-trimethyl-hexanoate.

Field of application: ONGRONOX INP 75D is an initiator for ethylene, vinyl chloride, vinylidenechloride, vinyl-acetate, acrylates etc. polymerization and copolymerization.

Information provided by BorsodChem Rt.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.875 g/cc
@Temperature 0.000 °C
Molecular Weight 314.5 g/mol
 
Thermal PropertiesOriginal ValueComments
Flash Point 43.0 °C
 
Descriptive Properties
Active Oxygen3.82
free acid content as isononanoic acid, max, %1
Hydrolyzable chlorine max 250 mg/kg
Peroxide, %75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mateck InP
Indium Phosphide, InP
Gallium Arsenide, GaAs
MarkeTech Indium Phosphide Semiconductor Wafer, Semi-Insulating Iron Doped, Czochralski-LEC Grown

PBORS16 / 27540

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.