MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Prodways PLASTCure Rigid 10 500 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Excellent detail resolution & sidewall quality Easy finishing Superior thermomechanical properties Low thermal expansion

Applications: Suitable for the manufacture of parts that require thermal stability, extreme accuracy and quick turnaround. Exceptional for parts designed for wind tunnel testing and unique applications in rapid tooling or high temperature testing, electrical casings, and automotive housings

Information provided by Genistar.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.60 g/cc
Water Absorption 0.50 - 0.70 %ASMT D570
Viscosity 900 - 1100 cP
@Temperature 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90 - 95
Tensile Strength at Break 50.0 - 65.0 MPaASTM D638
Elongation at Break 0.50 - 1.0 %ASTM D638
Tensile Modulus 7.70 - 8.20 GPaASTM D638
Flexural Strength 65.0 - 90.0 MPaASTM D790
Flexural Modulus 7.00 - 8.00 GPaASTM D790
Flexural Strain at Break 1.0 - 2.0 %ASTM D790
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 120 - 125 °CASTM D648
 
Descriptive Properties
AppearanceIvory opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DSM Somos® DMX-SL™ 100 Extremely tough/durable SL resin for stereolithography
DSM Somos® GP Plus 14122
DSM Somos® BioClear
3D Systems DuraForm® PA Nylon for SLS® Systems
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems

PPRODW907 / 172313

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.