MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound OF006A Polyphenylene Sulfide, Branched (PPS, Branched) (Americas)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: LNP THERMOCOMP OF006A compound is based on branched Polyphenylene Sulfide (PPS) resin containing 30% glass fiber.

Features: High Stiffness,Structural

Information provided by SABIC

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.58 g/ccASTM D792
 1.58 g/ccISO 1183
Moisture Absorption 0.0600 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm24hrs; ASTM D955
 0.0013 - 0.0030 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0040 - 0.0070 cm/cm24hrs; ASTM D955
 0.0040 - 0.0070 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 129 MPaASTM D638
 129 MPaISO 527
Elongation at Break 1.2 %ISO 527
 1.3 %ASTM D638
Tensile Modulus 12480 MPa1 mm/min; ISO 527
 12730 MPa50 mm/min; ASTM D638
Flexural Strength 193 MPaASTM D790
 220 MPaISO 178
Flexural Modulus 11250 MPaASTM D790
 11880 MPaISO 178
Izod Impact Notched 69.0 JASTM D256
Izod Impact, Unnotched 405 J/mASTM D4812
Izod Impact, Notched (ISO) 9.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 31.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 8.00 Jpeak; ASTM D3763
Impact Test 2.00 JMultiaxial Impact; ISO 6603
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 120 - 180 secASTM D495
Comparative Tracking Index 100 - 175 VUL 746A
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness >=1.50 mm
UL 746A
 60 - 120 sec
@Thickness >=3.00 mm
UL 746A
 >= 120 sec
@Thickness >=6.00 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 23.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 24.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 45.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 45.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 263 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 267 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 220 °CUL 746B
UL RTI, Mechanical with Impact 200 °CUL 746B
UL RTI, Mechanical without Impact 220 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.450 mm
UL 94
 5VA
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 320 - 330 °C
Zone 3 330 - 345 °C
Melt Temperature 315 - 320 °CInjection Molding
Mold Temperature 140 - 165 °C
Drying Temperature 120 - 150 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81751 / 289698

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.