MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-TH-22 High-Effective Rheological Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GY-TH-22 is a high-effective rheological additive which applies in many applications such as plaint, coating, printing ink, adhesives, sealants, resins.

Advantages:

  • Rheology and thixotropy control of liquid systems, binders, polymers, etc.
  • Used as anti-setting, thickening and anti-sagging agent
  • Reinforcement of HTV- and RTV-2K-silicone rubber
  • Improvement of free flow and anticaking characteristics of powders
Applications:
  • paints and coatings
  • road paints
  • various industrial and household paints
  • Unsaturated polyester resins, laminating resins and gel coats
  • HTV- and RTV-2K-silicone rubber
  • Adhesives and sealants
  • Printing inks
  • Cable compounds and cable gels
  • Plant protection
  • Cosmetics

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0900 g/ccTamper
Particle Size 45 µmSieve residue, ? 1.5%
pH 6.5
 
Component Elements PropertiesOriginal ValueComments
Loss on Ignition(%) 4.5 %
@Temperature 1000 °C,
Time 7200 sec
Sulfate, SO4 <= 1.5 %
 
Descriptive Properties
AppearanceWhite powder
Conductivity?1300 µS/cm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN416 / 266724

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.