MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Milliken® RenewWrap™ Primer Low viscosity epoxy primer
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: RenewWrap™ Primer is two-component, super low viscosity epoxy primer used to penetrate the pore structure of concrete substrates and to promote excellent adhesion for the RenewWrap FRP strengthening system.

Features and Benefits:

  • Super low-viscosity is ideal for penetrating surface pore structure of concrete substrates.
  • Cures to a solid with no shrinkage and bonds to all surfaces
  • 100% solids, solvent free system.
  • No VOC, low odor
  • Compatible with most substrates and with other constituent materials of the RenewWrap strengthening system.

Information provided by Milliken®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/cc
Viscosity 400 cP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 49.8 MPa
Elongation at Break 1.8 %
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 66.0 °C
 
Descriptive Properties
ColorAmberPart B
 AmberMixed
 ClearPart A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMILLIK048 / 195019

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.