Durez® 37113 is a liquid phenolic resin of the novolac-type, used in the refractory industry for the production of shaped and unshaped refractories. Addition of hexamethylenetetramine is necessary to make it thermosetting.Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |