MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Jilin Xingyun Chemical 4045 EPDM
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Property: Mooney viscosity proper; extraordinary fast cure rate; molecular weight distribution wide; ethylene content proper; process ability excellent; good comprehensive property

Application: Wire and cable etc. insulation profiles; sponge rubber; make tyre sidewall by blending with diene type series rubber; transparent rubber profiles; colorful rubber profiles and other various fast cure common rubber profiles.

Remarks: Very fast cure rate common rubber

Information provided by Jilin Xingyun Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.75 %
Mooney Viscosity 40 - 50
@Temperature 100 °C
ML 1+4
Ash <= 0.10 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 15.0 MPa
Elongation at Break >= 300 %
300% Modulus >= 10.0 MPa
 
Descriptive Properties
Content<10 ppmVanadium
 49-55%Ethylene
 6.7-8.7%ENB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJILINX013 / 317860

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.