MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
A. Schulman Diamond Centrex® 885 Profile Extrusion Grade  (discontinued **)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: Centrex 885 resin is a low-gloss ASA (acrylonitrile-styrene-acrylate) resin with good resistance to weather aging. It has good melt strength for profile extrusion and can be coextruded over polyvinyl chloride (PVC).

Applications: Typical applications for Centrex 601 resin include exterior siding, window frames and fences. As with any product, use of Centrex 885 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Weatherable Polymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Melt Flow 4.7 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 15.8 MPachs 0.2 in/min; ASTM D638
Tensile Strength, Yield 26.2 MPachs 0.2 in/min; ASTM D638
Flexural Strength 45.5 MPachs 0.05 in/min; ASTM D790
Flexural Modulus 1516 MPatangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 160 J/m
@Thickness 3.17 mm,
Temperature 23.0 °C
ASTM D256
Impact Test 17.0 J
@Temperature 23.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 107 °C
@Load 1.00 kg
120°C/hr; ASTM D1525
 
Optical PropertiesOriginal ValueComments
Gloss 3.0 %Extruded Strip; 60°; ASTM D523

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Appeel® 20D784 Ethylene Acrylate
Dow Appeel® LSR20D751 Lidding Sealant Resin
Fujipoly Industries Sarcon® NR-HTc Gap Filler Pad
INEOS Styrolution Luran® S 757G ASA
LyondellBasell Petrothene® LR734001 High Density Polyethylene, Sheet & Profile Extrusion Data

PDIAM359 / 126450

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.