MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Edinburg Plastics DOA006 PA 6/6 Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: Appearance: Colors

Processing Methods: Injection

Applications: Flame Retardant

Information provided by Edinburg Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccASTM D792-91
Linear Mold Shrinkage 0.0090 - 0.014 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 10500 psiASTM D638
Elongation at Break 5.0 %ASTM D638
Flexural Yield Strength 15000 psiASTM D790
Flexural Modulus 475000 psiASTM D790
Izod Impact, Notched 0.800 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 157 °CASTM D648
Flammability, UL94 V-0
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 249 - 260 °C
Middle Barrel Temperature 271 - 282 °C
Front Barrel Temperature 277 - 288 °C
Nozzle Temperature 277 - 288 °C
Melt Temperature 282 °C
Mold Temperature 60.0 - 88.0 °C
Drying Temperature 79.0 °C
Dry Time 4.00 - 8.00 hour
Moisture Content <= 0.20 %
Dew Point >= -40.0 °F
Back Pressure 40.0 - 100 psiLower is better
Screw Speed 30 - 70 rpmLower is better

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
Epsan Eplamid 66 GV0 30 NC Q1D0C001 Polyamide 66, Halogenated
Edinburg Plastics DOG056 PA 6/6 Flame Retardant, 25% Glass Filled
Bamberger Polymers Bapolene® 5062 Polypropylene, Injection Grade

PEDIN023 / 183526

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.