MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Microtherm Group MT Thermosphere® Moldable Insulation Paste
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material

Material Notes: MT Thermosphere® is a low density temperature resistant paste with excellent thermal insulation properties from cryogenic to high temperature exposure. It is a perfectly seamless insulation system. MT Thermosphere® is self drying and moldable. It dries by the evaporation of the water content. If required, it can be finished by painting or the application of a covering material.

Non-combustible to Euro Class A1 (DIN EN 13501-1:2002)

Hydrophobic at temperatures < 350ºC (662ºF) when set.

    Properties
  • Formulation based on glass microspheres in inorganic binder.
  • Capable of continuous single sided exposure to 650ºC (approx. 1200ºF).
  • Non-combustible to Euro Class A1.
  • Paste will air dry but drying can be accelerated by heating to no higher than 200ºC (approx. 390ºF).
  • No shrinkage when drying.
  • Good thermal insulation.
  • Low density / low weight.
  • Suitable for insulation of complex shapes in inaccessible areas.
  • Environmentally safe.
  • Hydrophobic.
    Applications
  • Typical application temperature range from -20 to 600ºC (approx. 0 to 1110ºF).
  • Precast shapes for pipes and difficult areas.
  • Penetration seals.
  • Gap sealing in insulation systems for continuity of protection.
  • On site repairs of existing insulation systems.
  • Any application where conventional insulation block or panel is difficult to use.

Information provided by Microtherm.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.110 g/ccdry
 0.330 g/ccwet
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.840 J/g-°C
Thermal Conductivity 0.0370 W/m-K
@Temperature -20.0 °C
@ 110 kg/m³; ASTM C177, ISO 8302, DIN EN-12667:2001-05
 0.0380 W/m-K
@Temperature 10.0 °C
@ 110 kg/m³; ASTM C177, ISO 8302, DIN EN-12667:2001-05
 0.0420 W/m-K
@Temperature 50.0 °C
@ 110 kg/m³; ASTM C177, ISO 8302, DIN EN-12667:2001-05
 0.0470 W/m-K
@Temperature 100 °C
@ 110 kg/m³; ASTM C177, ISO 8302, DIN EN-12667:2001-05
 0.0580 W/m-K
@Temperature 200 °C
@ 110 kg/m³; ASTM C177, ISO 8302, DIN EN-12667:2001-05
 0.0700 W/m-K
@Temperature 300 °C
@ 110 kg/m³; ASTM C177, ISO 8302, DIN EN-12667:2001-05
 0.0850 W/m-K
@Temperature 400 °C
@ 110 kg/m³; ASTM C177, ISO 8302, DIN EN-12667:2001-05
 0.102 W/m-K
@Temperature 500 °C
@ 110 kg/m³; ASTM C177, ISO 8302, DIN EN-12667:2001-05
Maximum Service Temperature, Air 650 °Cfor long term exposure
Shrinkage <= 2.0 %
@Temperature 450 °C,
Time 86400 sec
full soak
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature >=5.00 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant

CMICRO12 / 90054

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.