Teflon™ PTFE 8A X is a free-flowing white powder composed of relatively large particles and ideal for isostatic molding. Its most unique features are improved mold ability at lower pressure and improved surface smoothness of finished parts. It offers an excellent combination of properties that are characteristic of Teflon™ fluoroplastic resins. Teflon™ PTFE 8A X is often preferred for molding thick sheets and is sometimes used for ram extrusion of rod and tubing with thicker cross-sections. Properly processed products made from neat Teflon™ PTFE 8A X provide the superior properties typical of fluoroplastic resins. Many end products are fabricated from moldings of Teflon™ PTFE 8A X, such as: Ball valve seats, Seals, Discs, Lab ware, Pipe linings, Valves, Valve plugs, Ducting, Expansion bellows, Piston rings. Thick molded sheets are stock shapes made from Teflon™ PTFE 8A X.Information provided by Chemours. |