MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC XENOY™ 5220U PC+PBT (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
 1.21 g/ccASTM D792
Density 1.22 g/ccISO 1183
Water Absorption 0.50 %23°C/sat; ISO 62
Moisture Absorption 0.150 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0080 - 0.011 cm/cmSABIC method
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 15 g/10 min
@Load 5.00 kg,
Temperature 250 °C
cm³/10 min; ASTM D1238
 16 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50.0 MPa50 mm/min; ISO 527
 51.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 50.0 MPa50 mm/min; ISO 527
 53.0 MPa50 mm/min; ASTM D638
Elongation at Break 120 %50 mm/min; ISO 527
 120 %50 mm/min; ASTM D638
Elongation at Yield 4.0 %50 mm/min; ISO 527
 4.0 %50 mm/min; ASTM D638
Tensile Modulus 2050 MPa1mm/min; ISO 527
 2250 MPa50 mm/min; ASTM D638
 2250 MPa5 mm/min; ASTM D638
Flexural Yield Strength 80.0 MPa2 mm/min; ISO 178
 84.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2000 MPa2 mm/min; ISO 178
 2030 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 710 J/mASTM D256
 299 J/m
@Temperature -40.0 °C
ASTM D256
 530 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 50.0 kJ/m²80*10*4; ISO 180/1A
 30.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 55.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 60.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 120 - 180 secASTM D495
Comparative Tracking Index 400 - 600 VUL 746A
Hot Wire Ignition, HWI 15 - 30 secUL 746A
High Amp Arc Ignition, HAI >= 120 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 95.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 95.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 84.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 99.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 120 °CRate B/50; ISO 306
 122 °CRate B/50; ASTM D1525
 125 °CRate B/120; ISO 306
UL RTI, Electrical 75.0 °CUL 746B
UL RTI, Mechanical with Impact 75.0 °CUL 746B
UL RTI, Mechanical without Impact 75.0 °CUL 746B
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 255 - 270 °CInjection Molding
Zone 1 170 - 205 °CSheet Extrusion
 245 - 265 °C
Zone 2 195 - 255 °CSheet Extrusion
 250 - 270 °C
Zone 3 205 - 280 °CSheet Extrusion
 255 - 275 °C
Zone 4 205 - 280 °CSheet Extrusion
Adapter Temperature 225 - 280 °CSheet Extrusion
Die Temperature 230 - 280 °CSheet Extrusion
Melt Temperature 245 - 275 °C
 260 - 275 °C
Mold Temperature 65.0 - 90.0 °C
Roll Temperature 70.0 - 80.0 °CRoll Stack Temp - Top
 75.0 - 80.0 °CRoll Stack Temp - Middle
 80.0 - 95.0 °CRoll Stack Temp - Bottom
Drying Temperature 110 °CInjection Molding
 110 - 115 °CSheet Extrusion
Dry Time 4.00 - 6.00 hourSheet Extrusion
 4.00 - 6.00 hourInjection Molding
 8.00 hourCumulative; Sheet Extrusion
 8.00 hourCumulative; Injection Molding
Moisture Content 0.00 - 0.020 %
 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 50 - 80 %
Vent Depth 0.00130 - 0.00200 cm
Screw Speed 50 - 80 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF2UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10823 / 244290

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.