Wave Solder Flux #1010 is a versatile VOC-Free water-soluble wave flux that provides excellent solderability on difficult to solder assemblies. Wave Solder Flux #1010 is biodegradable and cleans to low ionic levels, leaving the assembly with high surface insulation resistance. Features: - Non-flammable
- High activity
- Wide process window
- Use with Pb-Free and Sn-Pb assembly process
Physical Properties - Color: Clear
- Flash Point: None
- Flux Classification Type: ORH1
Information Provided by Indium Corporation |