MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Radel® R-5500 Polyphenylsulfone (PPSU), Transparent
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Transparent, low flow for extrusion

Radel® R-5500 is a general purpose extrusion grade of polyphenylsulfone (PPSU), offering exceptional hydrolytic stability and better toughness than most commercially available high-temperature polymers. This resin has a high heat deflection temperature, excellent thermal stability, outstanding resistance to environmental stress cracking, good electrical properties and inherent flame retardant properties. Transparent and opaque colors are available.

Transparent Grades:
- Natural: Radel® R-5500 NT

Opaque Grades:
- Black: Radel® R-5500 BK937
- Bone: Radel® R-5500 NT15
- Grey: Radel® R-5500 GY1137
- Grey: Radel® R-5500 GY1037
- Grey: Radel® R-5500 GY874
- Red: Radel® R-5500 RD1018
- Orange: Radel® R-5500 OR1145
- Yellow: Radel® R-5500 YL1337
- Green: Radel® R-5500 GN1007
- Blue: Radel® R-5500 BU1027
- Blue: Radel® R-5500 BU391
- Violet: Radel® R-5500 VT2582
- Brown: Radel® R-5500 BN1164

Markets/Uses: Healthcare / Medical Devices / Case Handles and Brackets; Healthcare / Medical Devices / Dental Instruments; Healthcare / Medical Devices / Medical Reusable; Healthcare / Medical Devices / Medical Sheet Clear; Healthcare / Medical Devices / Medical Single Use Applications; Healthcare / Medical Devices / Medical/Healthcare Applications; Healthcare / Medical Devices / Orthopedics; Healthcare / Medical Devices / Packaging, Rigid Medical; Healthcare / Medical Devices / Sizing Trials; Healthcare / Medical Devices / Sterilization Cases, Trays and Lids; Healthcare / Medical Devices / Surgical Instruments; Membranes / Membranes / Food and Beverage Processing; Membranes / Membranes / Industrial Process Separations

Applications: Aerospace Applications; Aircraft Applications; Dental Applications; Food Service Applications; Hospital Goods; Medical Devices; Medical/Healthcare Applications; Membranes; Surgical Instruments

Features: Acid Resistant; Autoclave Sterilizable; Base Resistant; Biocompatible; Chemical Resistant; E-beam Sterilizable; Ethylene Oxide Sterilizable; Flame Retardant; Good Sterilizability; Good Thermal Stability; Heat Sterilizable; High ESCR (Stress Crack Resist.); High Heat Resistance; Hydrolytically Stable; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam Sterilizable; Ultra High Toughness

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccASTM D792
Water Absorption 0.37 %
@Time 86400 sec
ASTM D570
Water Absorption at Saturation 1.1 %ASTM D570
Linear Mold Shrinkage, Flow 0.0070 cm/cm
@Thickness 3.18 mm
ASTM D955
Melt Flow 12 - 17 g/10 min
@Load 5.00 kg,
Temperature 365 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 69.6 MPa
@Thickness 3.18 mm
ASTM D638
Elongation at Break 60 - 120 %
@Thickness 3.18 mm
ASTM D638
Elongation at Yield 7.2 %
@Thickness 3.18 mm
ASTM D638
Tensile Modulus 2340 MPa
@Thickness 3.18 mm
ASTM D638
Flexural Strength 91.0 MPa
@Strain 5.0 %,
Thickness 3.18 mm
ASTM D790
Flexural Modulus 2410 MPa
@Thickness 3.18 mm
ASTM D790
Izod Impact, Notched 690 J/m
@Thickness 3.18 mm
ASTM D256
Tensile Impact Strength 399 kJ/m²
@Thickness 3.18 mm
ASTM D1822
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 9.00e+15 ohm-cmASTM D257
Dielectric Constant 3.44
@Thickness 3.18 mm,
Frequency 60 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
@Thickness 3.18 mm
ASTM D149
 >= 200 kV/mm
@Thickness 0.0254 mm
ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 56.0 µm/m-°C
@Thickness 3.18 mm
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
Glass Transition Temp, Tg 220 °CASTM E1356
Flammability, UL94 V-0
@Thickness 0.760 mm
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.672ASTM D542
 
Processing PropertiesOriginal ValueComments
Zone 1 338 - 388 °CExtrusion
Zone 2 338 - 388 °CExtrusion
Zone 3 338 - 388 °CExtrusion
Zone 4 338 - 388 °CExtrusion
Zone 5 338 - 388 °CExtrusion
Adapter Temperature 327 - 371 °CExtrusion
Die Temperature 327 - 371 °CExtrusion
Melt Temperature 343 - 399 °CExtrusion
 360 - 391 °CInjection
Mold Temperature 138 - 163 °C
Drying Temperature 149 °C
@Time 9000 sec
 171 °C
@Time 14400 sec
Extrusion
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack; Clear/Transparent; Colors Available
FormsPellets
ProcessingBlow Molding; Extrusion; Film Extrusion; Injection Molding
 Machining; Profile Extrusion; Sheet Extrusion; Thermoforming
RoHS ComplianceYes
Screw Compression Ratio2.2:1.0
Steam Sterilization> 1000 Cycles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4395 / 280195

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.