ELASTOSIL® LR 6250 F is a free-flowing addition-curing silicone rubber, which is mixed with crosslinker to form a ready-to-use product with long pot life which cures rapidly at high temperatures. Special features: - solvent-free
- processing viscosity suitable for silk-screen printing
- long term flexibility over a temperature range from -50°C to +200 °C
- good resistance to chemicals
- long pot life of ready-to-use mixture
Application: ELASTOSIL® LR 6250 F may be used for applications which require high or low temperature resistant flexible coating.Information provided by Wacker. |