MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Shuman 211 Flame Retardant Polyphenylene Ether Copolymer Alloy
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Molded

Material Notes: Black, Custom Colors. Excellent flame retardancy, easy processability, good impact strength, good chemical resistance, injection molding and extrusion grades.

Data provided by the manufacturer.

Key Words: PPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccASTM D792
Melt Flow 1.5 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 116ASTM D785
Tensile Strength, Yield 47.0 MPaASTM D638
Izod Impact, Notched 1.60 J/cm1/8" Thick Specimen; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °CASTM D648
Vicat Softening Point 127 °CASTM D1525
Flammability, UL94 V-0
@Thickness 1.57 mm
 5VA
@Thickness 3.18 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 193 - 221 °CExtrusion
 221 - 260 °CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Iupiace® LN30 m-Polyphenylene Ether (m-PPE)
Polymer Resources PPX-FRG30 Modified-PPO, V-1 Flame Retardant, 30% Glass Reinforced
Mitsubishi Iupiace® LN60 m-Polyphenylene Ether (m-PPE)
Mitsubishi Iupiace® LN40 m-Polyphenylene Ether (m-PPE)
Mitsubishi Iupiace® GN30 m-Polyphenylene Ether (m-PPE)

PSHU05 / 67538

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.