MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Synthos SDH780 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Characteristics: SDH series is a special kind of linear thermoplastic Polyurethane Elastomer, which is designed for TPU Hot-melt film. It exhibits good toughness, wear resistance, elasticity and excellent bonding strength for TPU, PVC, Nylon, Polyester, fabrics, leather etc.

Applications: Toe-Puffs& Counters, hot-melt adhesive films and tapes, Fabric coatings, Seam Sealing Tapes, shoe materials, high-end interlining, heat transfer printing industry, textile, etc.

Information provided by Sundow Polymers Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 150 °C
ASTM D1238c
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength 20.0 MPaASTM D412
Elongation at Break 500 %ASTM D412
 
Processing PropertiesOriginal ValueComments
Cure Time 6.00 minTack-free time
 
Descriptive Properties
Flow-beginning temperature95°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSUNDOW126 / 320157

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.