MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Novec™ FC-4430 Fluorosurfactant
Categories: Fluid; Polymer; Thermoplastic; Fluoropolymer

Material Notes: 3M™ Novec™ Fluorosurfactant FC-4430 is a non-ionic polymeric fluorochemical surfactant belonging to a class of coating additives which provide low surface tensions in coating systems best served by fluorochemical surfactants. Novec fluorosurfactant FC-4430 contributes excellent wetting, spreading and leveling properties to a variety of coating systems.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/cc
pH 4.51% aqueous solution
Viscosity 2000 - 6000 cP
Vapor Pressure 0.0000930 bar
Surface Tension 1.5 dynes/cm0.5%, Light Phase: Cyclohexane
 2.2 dynes/cm0.5%, Light Phase: Heptane
 2.5 dynes/cm200 ppm, Light Phase: Cyclohexane
 3.2 dynes/cm200 ppm, Light Phase: Heptane
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg <= 0.000 °C
Flash Point 82.0 °CSetaflash closed cup

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
International Mold Steel Porcerax II Sintered, Porous Mold Steel
International Mold Steel Daido DRM2 Matrix High-Speed Steel

PMM33036 / 167783

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.