MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Evonik Vestodur® X9406 Black E70167 Impact Modified PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Impact Grade

Material Notes: Description: VESTODUR X9406 is an impact modified compound based on polybutylene terephthalate. The resin is used as a barrier layer resin in multilayer tubing 1000.1 (MLT 1000.1)developed by Degussa. MLT 1000.1 is a 3-layer-tubing comprising an outermost layer of VESTAMID LX9010, an adhesive layer of VESTODUR X9407, and an innermost layer of VESTODUR X9406. This MLT was developed as fuel line tubing with outstanding resistance against hydrocarbon permeation when alcohol containing fuels are used. VESTODUR X9406 provides excellent barrier properties also in contact with fuels at elevated temperatures.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccISO 1183
Water Absorption at Saturation 0.60 %ISO 62
Melt Flow 8.61 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 19.68 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ISO 1133
 73.8 g/10 min
@Load 10.0 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70ISO 868
Tensile Strength, Yield 40.0 MPaISO 527-1/2
Elongation at Break 40 %ISO 527-1/2
Elongation at Yield 3.8 %ISO 527-1/2
Tensile Modulus 1.75 GPaISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 140 µm/m-°C
@Temperature 23.0 - 80.0 °C
Longitudinal; ISO 11359, DIN 53752
CTE, linear, Transverse to Flow 140 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359, DIN 53752
Deflection Temperature at 0.46 MPa (66 psi) 145 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75-1/-2
Vicat Softening Point 145 °CMethod B, 50 N; ISO 306
 215 °CMethod A, 10 N; ISO 306

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestodur® X9407 Polymer Modified PBT
Evonik Vestodur® 3000 High Viscosity PBT
Evonik VESTAMID® MLT 1000.1 Nonconductive multi-layer tubes
BASF Ultradur® B 4520 BK00110 PBT

PHUMA75 / 47589

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.