MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC CYCOLOY™ FR Resin CX2244ME Polycarbonate + ABS (PC+ABS) (Americas)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: CYCOLOY CX2244ME Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is an injection moldable, medium flow, non chlorinated/brominated flame retardant grade. It has a UL94 V0@0.75mm and 5VB@1.5mm flame rating. This grade has improved chemical resistance compared to standard PC/ABS blends and is a good candidate for thin wall applications and hospital/medical equipment.

Features: Hydrolytic Stability,Chemical Resistance,Flame Retardant,Thin Wall,Non-Chlorinated,Non-Brominated,High Flow,Good Mold Release

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Density 1.20 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.100 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.20 %ISO 62-1
Viscosity 15 cP
@Load 2.16 kg,
Temperature 260 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 18 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50.0 MPa50 mm/min; ISO 527
 58.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 65.0 MPa50 mm/min; ASTM D638
 65.0 MPa50 mm/min; ISO 527
Elongation at Break 90 %50 mm/min; ISO 527
 100 %50 mm/min; ASTM D638
Elongation at Yield 4.0 %50 mm/min; ISO 527
 4.1 %50 mm/min; ASTM D638
Tensile Modulus 2600 MPa5 mm/min; ASTM D638
 2600 MPa1 mm/min; ISO 527
Flexural Strength 96.0 MPayield, 2 mm/min; ISO 178
 104 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2500 MPa1.3 mm/min, 50 mm span; ASTM D790
 2500 MPa2 mm/min; ISO 178
Izod Impact Notched 700 JASTM D256
 175 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 40.0 kJ/m²80*10*3; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Charpy Impact, Notched 40.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 65.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Strength 17.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 25.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 35.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 175 - 250 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness 0.750 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 0.750 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Hot Ball Pressure Test 75.0 °CPASS; IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 89.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 110 °CRate B/50; ASTM D1525
 110 °CRate B/50; ISO 306
 113 °CRate B/120; ISO 306
UL RTI, Electrical 90.0 °CUL 746B
UL RTI, Mechanical with Impact 90.0 °CUL 746B
UL RTI, Mechanical without Impact 90.0 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.750 mm
UL 94
 5VB
@Thickness >=1.50 mm
UL 94
 5VA
@Thickness >=3.00 mm
UL 94
Glow Wire Ignition Temperature 800 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 250 - 300 °C
Zone 2 240 - 290 °C
Zone 3 250 - 300 °C
Melt Temperature 250 - 300 °CInjection Molding
Mold Temperature 60.0 - 85.0 °C
Drying Temperature 80.0 - 90.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Vent Depth 0.00300 - 0.00750 cm
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80022 / 287969

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.