MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT TA-20 FG Silicone Defoamer
Categories: Other Engineering Material

Material Notes: Description: This is a food grade silicone defoamer emulsion formulated to control foam in food systems and processes.

Key Features

  • Highly active material based on silica-filled polydimethylsiloxane
  • Excellent foam knockdown and persistence characteristics
  • Effective in hot and cold systems
  • Effective in low concentrations
Key Applications
  • Vegetable washing
  • Food processing
  • Food starch and protein washes such as those found in egg and potato processing
  • Pickle manufacturing (brine solutions)
Application TA-20 FG is a water-dilutable, 20% active silicone defoamer, formulated to control foam in food systems and processes.

INCI Name: Simethicone

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 - 1.00 g/ccBS ISO 2781
Volatiles 76 %
Brookfield Viscosity 2000 cP
Storage Temperature 4.00 - 38.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceWhite liquid
IonicityNon-ionic
MIT FreeYes
Ultralow cyclic contentNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL235 / 314718

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.