MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Multibase Multi-Flex® TPE A 8620 BLK
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Formulated TPE compound is based on Shell's Kraton G resin and is widely used in automotive applications exhibiting a wide temperature range, replacing in many applications conventional thermoset rubber. Multibase is a licensed compounder for Shell's Kraton G polymers. Multi-Flex TPE contains Kraton™ G.

Data provided by Multibase.

Key Words: Thermoplastic Elastomer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccASTM D792
Linear Mold Shrinkage 0.012 cm/cmASTM D955
Melt Flow 3.0 g/10 min(Condition L) ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8710 sec; ASTM D-2240
Tensile Strength, Ultimate 10.3 MPaASTM D412
Elongation at Break 925 %ASTM D412
Flexural Modulus 0.137 GPamethod 1, Proc.B; ASTM D-790
Tear Strength 54.3 kN/mASTM D624

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 8620 Steel, mock carburized, reheated and oil quenched, 150°C (300°F) temper, 13 mm (0.5 in.) round
AISI 8620 Steel, double quenched and tempered (230°C (450°F)), carburized
AISI 8620 Steel, double quenched and tempered (150°C (300°F)), carburized
AISI 8620 Steel, direct quenched from pot, 230°C (450°F) temper, carburized
AISI 8620 Steel, direct quenched from pot, 150°C (300°F) temper, carburized

PLA084 / 49545

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.