MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Cabot BLACK PEARLS® 2000 Specialty carbon black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: General Description: BLACK PEARLS® 2000 carbon black is a very fine particle sized, super high surface area, conductive product with an extremely high structure. It is a furnace process carbon black designed for critical applications demanding excellent conductivity and good physical properties. BLACK PEARLS 2000 carbon black offers excellent conductivity and anti-static discharge properties at very low loadings in rubber compounds.

Performance Features: BLACK PEARLS 2000 carbon black has better electrical conductivity properties in rubber compounds than other Cabot conductive carbon blacks, VULCAN® XC-72, VULCAN® P and STERLING® C products. BLACK PEARLS 2000 carbon black is used in applications where other conductive carbon black products cannot meet the balance between conductivity and rubber property specifications. The percolation curve for BLACK PEARLS 2000 carbon black in rubber relative to other conductive carbon blacks can be found below. Rubber components having electrical resistivity in 103 to 106 ohm•cm range are normally classified as “antistatic” and components below 103 ohm•cm are classified as “conductive”. Rubber components made with BLACK PEARLS 2000 carbon black meet these conductivity requirements at relatively low carbon black loadings. BLACK PEARLS 2000 carbon black is also recommended for use in blends with other carbon blacks. The addition of a small percentage of BLACK PEARL 2000 carbon black can help to meet the required conductivity or anti-static level without the need for complex re-compounding without impacting other rubber properties. The rubber reinforcement properties of BLACK PEARLS 2000 carbon black are very high, well beyond the level offered by ASTM N100 and N200 type carbon blacks.

Typical Applications:

  • Antistatic and conductive applications
  • Hospital flooring and sheeting
  • Conveyor and power transmission belts
  • Hoses for mining, petroleum
  • Cable screening

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 73
@Temperature 100 °C
ML (1+4)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 63
Tensile Strength 17.0 MPa
Elongation at Break 560 %
100% Modulus 2.60 MPa
200% Modulus 4.80 MPa
300% Modulus 7.60 MPa
 
Descriptive Properties
Other Characteristics0.34Resilience, Zwick Rebound

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT008 / 315743

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.