Description: Cosmic D69 / 6130 is a long glass fiber filled, general purpose diallyl ortho phthalate molding compound which is supplied in a flake form. It can be easily molded in compression or transfer equipment and can be readily preformed for ease in handling. It can be stored at room temperature for two years without reducing performance. Features: D69 / 6130 combines the advantages of high impact strength, high insulation resistance, excellent compressive and flexural strength, and easy moldability. Applications: Structural parts, housings, terminals and insulators, or other applications requiring strength. Information provided by Cosmic Plastics Inc |