MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Shanghai Potomer Calcium Stearate
Categories: Other Engineering Material

Material Notes: CAS. 1592-23-0

Character: White powder, nontoxic, specific gravity 1.08, not dissolved in water, Dissolving point 148-155 Degree Celsius, dissolved in hot ethanol and aether.

Usage: 1. As stabilizer and lubricant of PVC, it is used in film of food package, medical, nontoxic soft products.
2. Along with basic lead salts and lead soap, it is used in rigid plastic products.
3. As lubricant and mould releasing agent, it is used in polyolefin and polyester to reinforce plastic and resins which are thermo-plastics.
4. As raw material, it is used in flatting agent of paint and core of pens making

Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Mesh Size 200 Mesh>95% aperture 0.075 ?screen
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 120 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content 2.0 %
 
Component Elements PropertiesOriginal ValueComments
Calcium, Ca 6.0 - 7.5 %
 
Descriptive Properties
Content<1%Dissociate acid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSPOTOM122 / 284568

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.