Polybilt 106 is compatible with a large variety of bitumens. For optimum results are preliminary study is recommended to determine the base bitumen grade and optimum Polybilt 106 content to achieve the desired end-use properties.- Raises binder softening point and decreases penetration
- Substantially improves resistance to rutting.
- Substantially improves resistance to jet fuels.
- Improves binder low temperature flexibility and cohesion.
Availability: Africa & Middle East and Europe Additive: Applications: Information provided by ExxonMobil |