MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Chengdu Letain PA6125 Blending (Alloy) Material
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Technical features: High stiffness and replacement of PA66; High-heat resistance; Parts of automobile and Parts of machines

Information provided by Chengdu Letain Plastic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccGB1033
Water Absorption 1.3 %GB1034
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 125 MPaGB1040
Elongation at Break 10 %GB1040
Flexural Strength 160 MPaGB9341
Izod Impact, Notched (ISO) 10.0 kJ/m²GB1043
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmGB1410
Surface Resistance 1.00e+13 ohmGB1410
Dielectric Constant 4.0
@Frequency 1000 Hz
GB1409
Dielectric Strength 30.0 kV/mmGB1408
Dielectric Loss Index 0.010
@Frequency 1000 Hz
GB1409
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 240 °CGB1634
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHENGLT006 / 255859

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.