MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin BN9003G Polyphenylene Ether + PS (PPE+PS) (Asia)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ BN0039 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This blow moldable grade exhibits a good balance of impact resistance and surface aesthetics. NORYL BN0039 resin, with its Low warpage and dimensional stability, is an excellent candidate for automotive exterior components including spoilers.

Features: Hydrolytic Stability,Low Creep Sensitivity,Low Warpage,Aesthetics & Visual effects

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
Density 1.06 g/ccISO 1183
Moisture Absorption 0.0500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.25 %ISO 62-1
Viscosity 12 cP
@Load 5.00 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0055 - 0.0075 cm/cmSABIC method
 0.0055 - 0.0075 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0055 - 0.0075 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 42.0 MPa50 mm/min; ASTM D638
 42.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 47.0 MPa50 mm/min; ISO 527
 48.0 MPa50 mm/min; ASTM D638
Elongation at Break 30.4 %50 mm/min; ISO 527
 45 %50 mm/min; ASTM D638
Elongation at Yield 3.4 %50 mm/min; ISO 527
 3.6 %50 mm/min; ASTM D638
Tensile Modulus 2170 MPa1 mm/min; ISO 527
 2240 MPa5 mm/min; ASTM D638
Flexural Strength 70.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 75.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2150 MPa1.3 mm/min, 50 mm span; ASTM D790
 2190 MPa2 mm/min; ISO 178
Izod Impact Notched 320 JASTM D256
 127 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched NBASTM D4812
Izod Impact, Notched (ISO) 25.0 kJ/m²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
 54.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 107 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 26.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 12.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 40.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 86.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 86.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 95.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 95.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 126 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 124 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 108 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 127 °CRate B/50; ISO 306
 130 °CRate B/120; ISO 306
 141 °CRate B/50; ASTM D1525
 
Processing PropertiesOriginal ValueComments
Zone 1 225 - 260 °CExtrusion Blow Molding
Zone 2 230 - 260 °CExtrusion Blow Molding
Zone 3 235 - 260 °CExtrusion Blow Molding
Zone 4 235 - 260 °CExtrusion Blow Molding
Zone 5 235 - 260 °C
Die Temperature 235 - 260 °CExtrusion Blow Molding
Melt Temperature 235 - 260 °CExtrusion Blow Molding
Head Temperature 235 - 260 °CZone 6 - Top Temperature
 235 - 260 °CZone 7 - Bottom Temperature
 235 - 260 °CZone 7 - Middle Temperature
Mold Temperature 65.0 - 95.0 °C
Drying Temperature 80.0 - 85.0 °CExtrusion Blow Molding
Dry Time 2.00 - 4.00 hourExtrusion Blow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82259 / 290206

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.