MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Cookson Group Plaskon® 1002 Conventional Encapsulant  (discontinued **)
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Test specimens were transfer molded and post cured 4 hours at 175°C.

A low cost, low stress, conventional molding compound recommended for high volume commodity-type packages that house simple linear and discrete devices. These packages include low lead count DIPs, TO-types, diodes and small SOICs. Excellent moldability (fast curing, minimal if any deflashing, no degreasing); Superior cosmetics and markability; Low stress

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.86 g/cc
Viscosity 16500 cP
@Temperature 175 °C
Automatic orifice Viscosity
Spiral Flow 63.0 - 87.0 cm177°C/1000 psi
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81
Flexural Strength 131 MPa
Flexural Modulus 17.0 GPa
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.8
@Frequency 1000 Hz
Dielectric Strength 16.0 kV/mm
Dissipation Factor 0.0020
@Frequency 1000 Hz
Arc Resistance 180 sec
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 °C
CTE, linear, Transverse to Flow 56.0 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.700 W/m-K
Glass Transition Temp, Tg 153 °C
Flammability, UL94 V-0
@Thickness 1.60 mm
 V-0
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 170 - 185 °CMolding temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultraform® H 4320 Q600 POM
Aremco Aremco-Bond™ 2340 High Temperature Epoxide Potting Compound
Master Bond EP42HT-2LTE Two Component Epoxy
BASF Ultradur® B 6550 PBT
BASF Ultradur® B 6550 LN PBT

PCOOK303 / 21399

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.