MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Tacolyn™ 3400 Resin Ester Dispersion
Categories: Polymer

Material Notes: Product Description: Tacolyn™ 3400 resin ester dispersion is an aqueous, 55% solids, solvent-free, anionic rosin ester dispersion prepared from a highly hydrogenated, high softening point resin. It is recommended for use in food packaging applications such as closures, lidding, and cold seal adhesives, as well as pressure sensitive adhesives that contact food. Tacolyn™ 3400 is also used in adhesives applications requiring higher temperature strength such as in high temperature masking tapes, packaging tapes, and contact adhesives.

Application/Uses:

  • Automotive
  • Building and Construction
  • Contact Adhesives
  • Pressure sensitive adhesives
  • Tapes and Labels
  • Waterborne Adhesives
Key Attributes:
  • APE-free
  • Direct food contact FDA clearances
  • Excellent thermal and UV stability
  • Good moisture resistance
  • Promotes high temperature performance

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/cc
Solids Content 55 %
Particle Size >= 225 µm
pH >= 7.0Tolerance Rang
 10
Brookfield Viscosity 1100 cP
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point 92.0 °CASTM E 28

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5598 / 222792

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.