MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parson Adhesives SONLOCK™ 3572 Anaerobic Thread Sealant
Categories: Polymer; Adhesive; Thermoset

Material Notes: SONLOK 3572 is a slow cure speed, low strength anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures rapidly in the absence of air between close fitting metal surfaces and provide low-pressure resistance immediately after application. SONLOK 3572 is ideal to seal against gases, water, LPG, hydrocarbons, oils and other chemicals. Excellent thixotropic property prevents migration of the sealant before or during curing.

Applications:

  • Ideal for locking and sealing of threaded metal pipes and fittings
  • Designed for coarse threads.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/cc
Brookfield Viscosity 17000 - 50000 cPRVT, Spindle 3 @ 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 70.0 psiSteel Pins & Collars; ISO 10123
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CASTM D696 K-1
Specific Heat Capacity 0.300 J/g-°C
Thermal Conductivity 0.100 W/m-KASTM C177
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -65.0 °F
Flash Point >= 100 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 6.00 - 8.00 hourFunctional
 24.0 hourFull
 45.0 - 60.0 minHandling
 
Descriptive Properties
ColorWhite
CompositionMethacrylate Ester
Initial Strength Retained (%)100Break Fluid for 500 hrs at 22°C
 100Break Fluid for 1000 hrs at 22°C
 65Water/Glycol for 1000 hrs at 87°C
 70Motor Oil for 500 hrs at 125°C
 70Motor Oil for 1000 hrs at 125°C
 90Gasoline for 500 hrs at 22°C
 90Gasoline for 1000 hrs at 22°C
 90Water/Glycol for 500 hrs at 87°C
 95Acetone for 500 hrs at 22°C
 95Acetone for 1000 hrs at 22°C
 95Ethanol for 500 hrs at 22°C
 95Ethanol for 1000 hrs at 22°C
Solvent ContentNone
Torque20 NmBreakloose, Pre-torqued to 5 Nm, M10 steel nuts and bolts, ISO 10964
 20 NmMax Prevail, Pre-torqued to 5 Nm, M10 steel nuts and bolts, ISO 10964
 3 NmPrevail, M10 steel nuts and bolts, ISO 10964
 7 NmBreakaway, M10 steel nuts and bolts, ISO 10964

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zircar Ceramics MICROSIL Microporous Insulation
Unifrax Excelfrax® 1800 Board Microporous Insulation
Saint-Gobain Korel® K40-30 Medium Deflection Micro-cellular Polyurethane Foam
Saint-Gobain Korel® K30-25 Soft Micro-cellular Polyurethane Foam
Saint-Gobain COHRlastic® R10470 Medium General-Purpose Silicone Sponge Rubber

PPARSN044 / 186487

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.