MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC VALOX™ 4012G PBT (Americas)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccASTM D792
Density 1.39 g/ccISO 1183
Water Absorption 0.20 %23°C/sat; ISO 62
Moisture Absorption 0.0700 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cmSABIC method
 0.0060 - 0.016 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cmSABIC method
Melt Flow 9.0 g/10 min
@Load 1.20 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 10 g/10 min
@Load 1.20 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 117 MPaISO 2039-1
Tensile Strength at Break 72.0 MPa5 mm/min; ISO 527
 75.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 72.0 MPa5 mm/min; ISO 527
 75.0 MPa5 mm/min; ASTM D638
Elongation at Break 3.0 %5 mm/min; ASTM D638
 4.0 %5 mm/min; ISO 527
Elongation at Yield 3.0 %5 mm/min; ASTM D638
 4.0 %5 mm/min; ISO 527
Tensile Modulus 4500 MPa1mm/min; ISO 527
 4600 MPa5 mm/min; ASTM D638
Flexural Strength 110 MPa2 mm/min; break; ISO 178
Flexural Yield Strength 110 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3500 MPa2 mm/min; ISO 178
 3940 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 74.0 J/mASTM D256
 74.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 6.00 kJ/m²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 37.0 kJ/m²80*10*4; ISO 180/1U
 37.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 45.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 45.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 4.00 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 25.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 30.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
Dissipation Factor 0.0010
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.014
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 150 VIEC 60112
 250 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 60.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 85.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 215 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 170 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 175 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 205 °CRate B/50; ASTM D1525
 205 °CRate B/50; ISO 306
 208 °CRate B/120; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
UL 94 by SABIC-IP
Glow Wire Test 750 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 60.0 °CHopper Temperature
Nozzle Temperature 240 - 260 °CInjection Molding
Zone 1 230 - 245 °C
Zone 2 240 - 255 °C
Zone 3 245 - 265 °C
Melt Temperature 250 - 270 °C
Mold Temperature 40.0 - 100 °C
Drying Temperature 110 - 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10255 / 243722

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.