Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 15% sinusoidal Fiberglass Side 2: Cured Fusible Silicone Rubber Interleave: Polyester Film FAR 25.853 Recognition: Product is designed to meet the FAR 25.853 App. F, P.1,.Aii flame resistance requirements but is not recognized by an FAA test Laboratory. UL94V-0: The product is designed to meet UL94V-0 flame resistance requirements but is not recognized by Underwriters Laboratories. This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications. Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation. |