MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX™ Resin GTX626 Polyphenylene Ether + PA (PPE+Nylon)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 626 resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This blow moldable and extrudable grade exhibits high heat resistance and excellent chemical resistance. NORYL GTX626 resin may be an excellent candidate for exterior automotive applications such as wheel covers and wheel trim.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,High Heat Resistance,Low Warpage

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.013 - 0.014 cm/cm
@Thickness 3.20 mm
SABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 62.0 MPa50 mm/min; ASTM D638
Elongation at Break 83 %50 mm/min; ASTM D638
Flexural Strength 95.0 MPayld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2270 MPa2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 336 JASTM D256
 122 J
@Temperature -30.0 °C
ASTM D256
Dart Drop, Total Energy 31.0 Jpeak; ASTM D3763
 36.0 J
@Temperature -30.0 °C
peak; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 179 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 1 270 - 280 °CExtrusion Blow Molding
Zone 2 270 - 280 °CExtrusion Blow Molding
Zone 3 270 - 280 °CExtrusion Blow Molding
Zone 4 270 - 280 °CExtrusion Blow Molding
Zone 5 275 - 290 °C
Die Temperature 275 - 290 °CExtrusion Blow Molding
Melt Temperature 275 - 290 °CExtrusion Blow Molding
Head Temperature 275 - 290 °CZone 6 - Top Temperature
 275 - 290 °CZone 7 - Bottom Temperature
Mold Temperature 80.0 °C
Drying Temperature 80.0 °CExtrusion Blow Molding
Dry Time 4.00 hourExtrusion Blow Molding
 16.0 hourCumulative; Extrusion Blow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82126 / 290073

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.